Traditional proofing simulation printing Heavy Duty Paper Bags With Handles

Feb 24, 2023

Leave a message

Traditional proofing simulation printing Heavy Duty Paper Bags With Handles

 

Proofing is the bridge between platemaking and printing. Its quality directly affects the quality of plate-making and printed matter.

At present, there are many ways of color proofing, and gradually from the traditional proofing to digital but traditional machine proofing. The following is an analysis of some common problems in the traditional machine proofing.

 

1. Excessive network expansion

Especially in summer, the indoor temperature is too high, if there is no air conditioning equipment, it will inevitably cause the increase of ink fluidity, the general solution is to add 2% extra oil in ink, so that the viscosity of the ink increases; The version of the refrigeration temperature is appropriate to reduce 1 ~ 2℃, increase the coagulation force of ink, so that the increase rate of dot will be improved.

 

In addition, there are several factors causing the increase of dot, should pay attention to master.

 

(1) plate pressure is too large. Table pressure is best in the range of 0.1 ~ 0.11mm, and the paper table pressure should be in the range of 0.12 ~ 0.13mm, which is good for improving dot increase.

 

(2) rubber blanket aging. The rubber blanket is used for too long, the surface is oxidized, the elasticity is weakened, and the surface is smooth. With such rubber cloth proofing, ink absorption is poor, transfer performance is not good, will inevitably cause too much dot increase. Therefore, it is necessary to replace the new rubber blanket in time.

 

(3) the ink roll pressure is too large, the ink roll aging, the ink roll itself can not grasp the ink. The roller pressure should be timely adjusted according to the standard. The pressure between the roller and the plate should be adjusted to 6mm, and the pressure between the roller and the serial roller should be adjusted to 4mm. And timely replacement of ink roller.

 

(4) too much ink. Sometimes due to the shallow version, in order to recover the original manuscript, not according to the standard data operation, too much to increase the amount of ink, resulting in excessive dot increase. Therefore, in any case, we should strictly operate according to the standard data, can not borrow deep, borrow shallow, original too shallow should improve the original.

 

(5) excessive moisture. If the water is too large, the ink will not be printed. If you want to print the ink, the ink will be diluted and the amount of ink will be increased, which will inevitably cause the dot to increase too much. Therefore, moisture must be controlled during operation.

 

(6) version of the refrigeration temperature is too high, refrigeration does not work, so the ink can not be condensed, large mobility, resulting in excessive dot increase. Timely adjust the refrigeration equipment, master the flow of ink.

 

2. The network is hollow

Sometimes the sample dot increases too small, dim sum appears hollow, this situation has the following reasons.

 

(1) winter due to the indoor temperature is low, relative humidity is small, operation, printing plate table refrigeration is too low, ink viscosity is large, ink on the plate due to cold and solidification, rubber blanket in the transfer of ink, the ink on the plate is pulled up around the center is pulled back to the plate, resulting in the dot center has a small white spot.

 

(2) PS version rough, sand is too thick.

 

(3) inappropriate pressure, etc.

 

The solution is:

(1) the temperature of the plate can be appropriately raised.

 

(2) Add 5% diluent in the ink, so that the ink moist and flow degree is appropriate.

 

(3) to choose uniform sand, thickness and depth of appropriate PS plate.

 

3. Proof is not glossy

Proof dull is mainly caused by hard ink, small fluidity, insufficient ink, low color saturation. The solution is:

 

(1) The use of "8" font ink, can be added in the four main color 5% of the diluent, so that the gloss of the proof can be improved.

 

(2) the amount of ink to play enough to achieve the best field density, the proof will be glossy.