Printing Paper Turntable Board Table Game Resin Plate Making Six Common Problems
May 22, 2023
Leave a message
Printing Paper Turntable Board table Game resin plate making six common problems
Photosensitive resin plate is a synthetic polymer material as a film forming agent, unsaturated organic compounds for photocrosslinking agent, and the production of a photosensitive relief plate. Almost all photosensitive resin plates are illuminated by light (mainly ultraviolet), resulting in cross-linking between molecules to form a relief image with some kind of insolubility. Photosensitive resin plate from the process can be divided into solid type and liquid type two. By the combination of saturated sexy light resin solid type series prefabricated plate material cost is relatively high, but the quality is better, you can make commodity packaging, trademark plate, network cable plate; Composed of unsaturated polyester resin liquid type series that coated plate (simply said is used to prepare a sensitive liquid for the base production, and then coated with resin, sensitive and production) the price is relatively low, suitable for rough text line version.
In the actual operation of solid resin plate plate making process often appear the following problems, only comprehensive analysis, different treatment, to find out the root of the problem, in order to solve the problem.
A, resin version of the text, lines, pattern lines are too thin, too small, small characters and independent points fall off, small lines curved
In the resin plate making, the common thin line bending and small text, independent point off and other problems.
The main reasons are:
l, resin version exposure time is insufficient;
2, the negative contrast is small, gray fog, not clear;
3, baking resin version and heat curing processing is improper;
4, brush resin version when the water temperature is low, washing time is long, brush bristles, brush version is too deep;
5, printing pressure is too large, adjustment is not appropriate.
Solution:
1, in the resin version, encounter small text, lines, patterns, independent points, to master the correct exposure time. The exposure time of 3kw iodogallium lamp is about 20min. The exposure time must be extended compared with the normal version, so that the small lines, words and independent points can stand and not fall off. Due to the long exposure time, the resin version of the mesh side and the slope is smaller (about 70°), text and text base firmly.
2, baking resin version, drying and heat curing treatment, under normal circumstances, oven temperature control at 60 to 80 degrees Celsius, the purpose is to version of the water evaporation; Dry temperature is too high, resin version is easy to foam.
3, the operator darkroom technology is required to be strong, film processing contrast should be as far as possible, no fog, text, smooth lines, no lack of pen break.
4, in the production of solid resin version, whether it is automatic plate making machine brush version, or manual brush version, the water temperature should be controlled at 50-60 ℃, washing until the base is exposed. Brush resin version to rotate the brush, brush on one side of the version, easy to side and slope brush, resulting in small lines of bending, off; Brush version to choose those hair soft suitable brush, if the bristles are hard, it will make small text brush fall damage; Brush resin version should pay attention to mastering the depth of the version brush, brush version does not have to wash the bottom base, brush version too deep easy to version of the text, lines, patterns are brushed off, in addition, pay attention to the brush version of the rinse time is not too long.
5, resin plate live on the machine printing, to adjust the pressure between the ink roller and resin plate, resin plate and embossing cylinder, resin plate printing pressure is smaller than the adjustment of copper zinc plate, printing type pressure. Avoid due to excessive pressure, inking rollers and embossing rollers to the resin version of the fine text lines to crush, affecting its printing resistance.
Two, text, line version in the resin version blurred
The main reasons are:
1. Excessive exposure;
2, the vacuum adsorption is not solid in the sun;
3, film contrast is small, not clear.
The solution:
1, the mastery of the resin version of the exposure time, especially the hollow text, the line is the easiest paste version, the design of text and text as far as possible a little thicker.
2, printing machine suction to firm. If the inspiration is not real, there is a gap between the resin version and the film, UV rays will be shot from around, resulting in photosensitive paste version.
3, before printing, we should carefully check whether apricot film paste version, good light transmittance, contrast, clear, in order to meet the needs of plate quality.
Three, resin version scour immovable
The main reasons are:
l, resin version of the plate has exceeded the shelf life, or any production, storage, transportation in the process of light leakage, resin version sensitive hardening;
2, washing version of the water temperature is too low;
3, film darkroom processing is not good, negative light poor, small density.
The solution:
1, resin version storage period is about half a piece, printing manufacturers should be based on the production capacity and consumption of the factory to buy, do not blindly buy too much, otherwise it will cause overdue failure.
2, resin version is sensitive material, the most afraid of production, storage, transportation link light leakage. Save the resin version, the plate should be temporarily not used in a sealed box, sealed with a black plastic bag; Resin version should be placed in a dry, moisture-proof place.
3, brush version of the water humidity control at about 60-70℃. The water temperature is too low, will affect the unsensitive resin film after water dissolution; At higher temperatures, dissolution is accelerated. [next]
Four, the resin version of the piece pattern or scars
The main reasons are:
1, between exposure, resin version is not coated with a small amount of talcum powder, corn starch, resulting in the contact between the negative and resin version is not close, there are bubbles;
2, printing machine vacuum pump suction is not real;
3, the film transparent temple is not smooth, there is gray fog.
The solution:
1, in the resin version of the surface coated with trace talcum powder, corn starch, its purpose is to prevent the page of resin adhesion negative, resulting in suction is not solid. The resin plate with a trace of fine particulate matter, can solve the problem.
2. After the printing machine is used for a period of time, it is necessary to overhaul in time, fill vacuum oil, clean up the dust and paper wool in the wall of the suction rubber tube, and the suction volume of the vacuum pump is generally 30-40m3 / h.
3, the film transmission performance is good, pay attention to exposure, development time, fixing, washing to be thorough, so that the negative no fog, no yellowing.
Five, resin version curling, dry crack
The main reasons are:
1, drying and heat curing time is too long;
2. Excessive post-exposure (fill light);
3, plate material expired or there are quality problems.
The solution:
1, resin version drying and heat curing treatment time can not be too long. As long as the layout is dry and the curved lines become straight.
2, after exposure (fill light) after drying, hot curing treatment, can not be excessive fill light, otherwise easy to make the resin hard and brittle. Just watch the page change from green to light red to ancient yellow. Encountered plate crimp serious, can be put into the water soaking 5-10min, and then dry.
3, plate material when using to recognize the production date, expired metamorphic plate material easy to curl, should not be used again.
Six, the printed text is incomplete
The main reasons are:
1, printing machine glass plate dirty serious;
2, the backplate painting ink stained the graphic part of the negative, the red tear film fragments of the plate falling into the negative;
3, brush version when too much force, brush bristles too hard.
The solution:
1. Develop good working habits of civilized and safe production. Before printing, the dust, oil, ink, paper and other dirty dirt inside and outside the glass plate of the printing machine is cleaned with water or cotton dipped in alcohol.
2. Be careful when painting ink on the negative, do not paint the picture and text. After the ink is dry, you can print the plate again.
3, brush resin version, force should be uniform, first heavy after light; Don't brush too hard. At the same time, it is also necessary to prevent hard objects from scratching the page and causing damage.